The loss of stability of the wetting water films on the quartz surface with increasing temperature was found. It is assumed that this is due to the temperature dependence of the structure of water in the ...
A technological complex has been developed to remove clay minerals, iron oxide and fractions heavier than 2.9 t / m3 from glass quartz sands. The basis of the circuit diagram of the apparatus of the complex ...
A device for determining the wettability of quartz sand has been developed. It is shown that with an increase in temperature, the surface wettability of the minerals included in the composition of glassy ...
For deferrization of substandard sands with a mass content of 0.34% Fe2O3, a method of flotation with a steam-air mixture was used according to the scheme "in two jets": from & frac12; parts of ...