The efficiency of iron removal in the biochemical method of kaolin processing depends on the particle size of iron minerals, their magnetic properties and structural organization - weakly crystallized ...
The efficiency of iron removal from kaolin increases with the inclusion of iron bioreduction in the technological scheme. The process can be accelerated by a combination of factors of humidity and temperature ...
The flowchart of a two-stage method for removing iron from the composition of porcelain stone is presented: with a combination of bio- and chemical reduction of iron under conditions of stagnant and water ...
The spectrocolorimetric and luminescent characteristics of porcelain containing neodymium oxide additives have been studied. It has been shown that an increase in whiteness occurs when the content of neodymium ...
Colorimetric identification of porcelain items by the type of material is reduced to finding the classification functions obtained on the training sample and linking the color coordinates with the type ...
A technology for the production of gypsum-ceramic material based on fluoroanhydrite has been developed. With the help of methods of physicochemical analysis, its composition and properties are determined. ...
The effect of the content of water vapor and oxygen in the atmosphere of a tin molten bath on the microhardness of the surface layers of float glass from various enterprises in Russia and Ukraine has been ...