The results of studies on the replacement of clay raw materials of the Ukrainian field with Nizhneuvelskaya clay (Russia) in the composition of the ceramic mass are presented. The physicochemical properties of the developed mass have been determined. Ceramic products were obtained at a firing temperature of 1070 ° C with a water absorption of no more than 3% and a total linear shrinkage of less than 13%. Tab. 6, bibliography: 3 titles.
Yugai N.S., Klimova E.V. Rheological properties of majolica slip with a thinning additive based on sodium polyacrylate. 2004. N 1. S. 19 - 21.
Dobrovolsky A. G. Slip casting. 2nd ed., Rev. and add. Moscow: Metallurgy, 1977.240 p.
Technological tests of clays: textbook. manual / ed. A. V. Ivanova, N. A. Mikhailova. Ekaterinburg: Publishing house of GOU VPO USTU-UPI, 2006.45 p.
The article can be purchased
electronic!
PDF format
Not on sale
UDK 666.32
Article type:
Science for ceramic production
Make a request