It was found that the use of a new MB1 organic bond with a 45/38 micron grinding powder instead of an M2-01 bond with a 30/40 micron micropowder made it possible to increase the productivity of the final diamond grinding of high-quality and art glass without subsequent chemical polishing by 2 - 2.5 times and reduce the roughness of the treated surface by 20% while increasing the specific consumption by 14 - 28%. Il. 2, bibliography: 2 titles.