The change in some parameters of the nanoscale coating under the action of 0.1 N solutions of hydrochloric and nitric acid has been studied. It was found that the swelling in hydrochloric acid is more intense than in nitric acid. The intensity of dissolution of a nanosized coating in a 0.1 N solution of nitric acid is directly proportional, and in hydrochloric acid is inversely proportional to the duration of etching.
Atkarskaya A.B. Changes in the characteristics of nanosized coatings under the action of hydrochloric acid solutions. 2012. N
9.P. 37 - 41. Atkarskaya AB Changes in nanosize coatings by sulfuric acid solutions // Glass and ceram. 2013. V. 69. P. 313 - 317.
Rabinovich VA, Khavin Z. Ya. Short chemical reference book. L .: Chemistry, 1978.392 p.